Process
After leaving printed specimen to dry inside the tank for at least three days, it is excavated by hand and excess powder is removed using brushes. The brushed specimen was then left to dry for four more days.




Process: Firing in Kiln









Height of Specimen: 8 cm
Nozzle Diameter: 8 cm
Tool: Lutum Piston
Air Pressure: 3-4 bar
Speed: 9 mm/sec

Height of Specimen: 8 cm
Nozzle Diameter: 8 cm
Tool: Lutum Piston
Air Pressure: 3-4 bar
Speed: 9 mm/sec